Laser surface treatment of AZ91 magnesium alloy presprayed with WC–Co B Mehrjou, R Soltani, MH Sohi, MJ Torkamany, Z Valefi, H Ghorbani Surface Engineering 32 (12), 893-901, 2016 | 13 | 2016 |
Microstructural and mechanical investigations on the heat treatment rejuvenation of a long-term service-exposed GTD-111 Ni-based superalloy A Geranmayeh, M Malekan, F Forghani, H Ghorbani Materials Science and Engineering: A 862, 144381, 2023 | 11 | 2023 |
Material characterization of long-term service-exposed GTD-111 nickel based superalloy H Ghorbani, H Farhangi, M Malekan Engineering Failure Analysis 148, 107061, 2023 | 9 | 2023 |
Liquid Phase Surface Treatment of Ti-6Al-4V Titanium Alloy by Pulsed Nd: YAG Laser H Ghorbani, M Heydarzadeh Sohi, MJ Torkamany, B Mehrjou Journal of Materials Engineering and Performance 24, 3634-3642, 2015 | 5 | 2015 |
Microstructural investigation and creep behavior of long-term exposed directionally solidified GTD-111 nickel based superalloy H Ghorbani, H Farhangi, M Malekan Materials Science and Engineering: A 890, 145811, 2024 | 1 | 2024 |
In-situ synthesis of TiC/Ti alloyed layer via pulsed Nd: YAG laser melting of Ti-6Al-4V titanium with preplaced carbon-based powder H Ghorbani, MS Khorrami, A Geranmayeh, MH Sohi Optics and Lasers in Engineering 172, 107864, 2024 | 1 | 2024 |
Microstructure and mechanical properties of titanium matrix composite reinforced by functionalized MultiWalled Carbon Nanotube H Ghorbani, A Habibolahzadeh, M Azadeh, A Kariminejad Advanced Materials Research 829, 530-533, 2014 | 1 | 2014 |
Liquid phase surface treatment of Ti-6Al-4V titanium alloy pre-sprayed with TiC/Ni using pulsed Nd-YAG laser H Ghorbani, M Heydarzadeh Sohi, MJ Torkamany Advanced Materials Research 829, 525-529, 2014 | 1 | 2014 |
Control of microstructure and solidification cracks in laser powder bed fusion additive manufacturing of high-strength aluminum alloys A Gandomdoust, MS Khorrami, SF Kashani-Bozorg, H Ghorbani Journal of Welding Science and Technology of Iran 9 (1), 39-57, 2023 | | 2023 |
Microstructural Characterization and Damage Mechanism of the First Stage Blade GE MS9001 After Long-term Exposure H Ghorbani, H Farhangi, M Malekan Journal of New Materials Spring 14 (51), 2023 | | 2023 |
Mechanically Activated synthesis of Tungsten Carbide Nanoparticles from Tungsten Oxide A Kariminejad, B Ghasemi, M Milani, H Ghorbani, M Azadeh Advanced Materials Research 829, 622-626, 2014 | | 2014 |